來源:http://lvuee.com/ 日期:2022-07-30 發布人:
經過多年的推廣,水泥就地冷再生技術被業內人士所熟知,并經常加以應用,看似簡單的水泥就地冷再生工藝,對于質量把握方面實際并不簡單,理由如下:
After years of promotion, the cement in situ cold regeneration technology is well known by people in the industry and is often applied. The seemingly simple cement in situ cold regeneration process is not simple in terms of quality assurance. The reasons are as follows:
1、冷再生工藝有其適用性,先期路面診斷很必要。水泥就地冷再生工藝一般是對原路面進行銑刨、整平、碾壓再成層的施工技術,他只是對于淺層(不大于25cm)路面結構的再生利用,所以對于路面結構下層的病害沒有修復作用。對于路面基層承載力不足,彎沉值過大等情況需要進行深層處理以恢復路面的使用功能,簡單的一層冷再生工藝不能起到長效的效果。
1. The cold regeneration process has its applicability, so it is necessary to diagnose the pavement in advance. The cement in situ cold recycling process is generally the construction technology of milling, leveling, rolling and re layering the original pavement. It is only the recycling of the shallow (no more than 25cm) pavement structure, so it has no repair effect on the diseases of the lower layer of the pavement structure. For the insufficient bearing capacity of the pavement base and the excessive deflection value, deep treatment is needed to restore the use function of the pavement, and the simple one-layer cold regeneration process cannot have a long-term effect.
2、冷再生層級配的檢測與調整會影響到再生層的質量。冷再生層根據原有路面的結構有灰土基層的冷再生、二灰碎石基層冷再生與水穩碎石基層冷再生。對于灰土基層的冷再生一定要慎重,建議只當路面底基層使用。相同水泥劑量情況下,路面基層級配合適與否直接影響其強度,所以經篩分不滿足級配要求的銑刨料須添加新料進行調整。
2. The detection and adjustment of the cold regeneration layer configuration will affect the quality of the regeneration layer. According to the structure of the original pavement, the cold regeneration layer includes the cold regeneration of lime soil base, lime fly ash macadam base and water stabilized macadam base. We must be careful about the cold regeneration of lime soil base, and it is recommended to use it only for the subbase of the pavement. Under the condition of the same cement dosage, whether the gradation of pavement base is appropriate or not directly affects its strength, so the milled materials that do not meet the gradation requirements after screening must be adjusted by adding new materials.
3、水泥劑量的確定也會直接影響到再生層的質量。適宜的水泥劑量不僅可以避免因水泥劑量不足而導致的強度不足現象,而且可以減少因水泥劑量過大而造成的基層應力收縮裂縫現象,延長道路的壽命。
3. The determination of cement dosage will also directly affect the quality of regeneration layer. Appropriate cement dosage can not only avoid the phenomenon of insufficient strength caused by insufficient cement dosage, but also reduce the phenomenon of stress shrinkage cracks caused by excessive cement dosage and prolong the service life of the road.


4、水泥的選用關重要。水泥冷再生并不是使用任何水泥都可以,它有嚴格的要求。它對水泥結合料的要求基本與水泥穩定碎石對水泥的要求相同,需要初凝時間大于3小時,終凝時間大于6小時的緩凝水泥。
4. The selection of cement is very important. Cold recycling of cement is not possible with any cement. It has strict requirements. Its requirements for cement binder are basically the same as those for cement stabilized macadam, requiring retarded cement with initial setting time of more than 3 hours and final setting time of more than 6 hours.
5、施工用水的選擇。看似無關緊要的因素,但可能因使用雜質過多或鹽離子過多的施工用水,致使工程質量出現問題。
5. Selection of construction water. Seemingly insignificant factors, but there may be problems in the project quality due to the use of excessive impurities or salt ions.
6、冷再生機租賃人員認為水泥攤鋪的均勻程度直接影響強度的均勻性。
6. The leasing personnel of the cold recycling machine believe that the uniformity of cement paving directly affects the uniformity of strength.
7、合理的整平時機會影響再生層的內在質量。一般再生機自重都較重,再生后兩輪間與輪跡處密實度會存在很大的差異性,如何此間差異性后再刮平直接會影響到再生層內部密實度的均勻性。
7. Reasonable leveling will affect the internal quality of the regeneration layer. Generally, the self weight of the regenerator is heavy, and there will be great differences in the compactness between the two wheels and the wheel trace after regeneration. How to eliminate this difference and then scrape it will directly affect the uniformity of the compactness inside the regeneration layer.
水泥冷再生施工工藝做好并不容易,并不是任何一個施工隊伍都能夠嚴格把控的,所以在施工過程選用,規范的作業隊伍是保障工程質量的前提。更多相關信息獲取就來我們網站http://lvuee.com看看吧。
It is not easy to do a good job in the construction process of cement cold recycling, and not any construction team can strictly control it. Therefore, the selection of professional and standardized operation teams in the construction process is the premise to ensure the project quality. Come to our website for more information http://lvuee.com Take a look.
下一篇:如何正確操作小型壓路機是關鍵 上一篇:使用路拌機時應該提前做好一切準備
閱讀/ Recommended reading
- 冷再生機租賃:現場瀝青路面冷再生機用于瀝青混凝土路面的銑刨以及添加瀝青、水等材料后的舊瀝青路面的再生。 2026-01-19
- 冷再生機租賃:率、多用途助力公路基層底層穩定土現場就地拌和作業 2026-01-16
- 冷再生機租賃:淺析冷再生技術的使用現狀及存在問題 2026-01-14
- 冷再生機租賃:道路冷再生時粒徑過大該怎么處理 2026-01-13
冷再生機租賃:水泥就地冷再生施工方法
[2026-01-21]
一、施工步驟 1、 Construction steps (一)施工準備 (1) Construction preparation 需要冷再生施工的路面要平坦,如有大...